levermaat (mm) |
schone maat (mm) |
CuSn7Zn4Pb7-C (CC493K) |
CuSn12-C (CC483K) |
ca kg/m |
13 | 12 | ✔ | ✔ | 1,2 |
15 | 14 | ✚ | 1,5 | |
16 | 15 | ✔ | ✔ | 1,8 |
17 | 16 | ✔ | 2,0 | |
19 | 18 | ✔ | ✚ | 2,5 |
21 | 20 | ✔ | ✔ | 3,0 |
23 | 22 | ✔ | ✔ | 3,6 |
26 | 25 | ✔ | ✔ | 4,8 |
29 | 28 | ✚ | 5,9 | |
31 | 30 | ✔ | ✔ | 6,6 |
levermaat (mm) |
schone maat (mm) |
CuSn7Zn4Pb7-C (CC493K) |
CuSn12-C (CC483K) |
ca kg/m |
33 | 32 | ✔ | 7,6 | |
36 | 35 | ✔ | ✔ | 9,0 |
41 | 40 | ✔ | ✔ | 11,7 |
46 | 45 | ✔ | ✔ | 14,7 |
51 | 50 | ✔ | ✔ | 18,1 |
56 | 55 | ✔ | ✔ | 22,0 |
61 | 60 | ✔ | ✔ | 26,0 |
66 | 65 | ✔ | ✔ | 30,4 |
71 | 70 | ✔ | ✔ | 35,2 |
levermaat (mm) |
schone maat (mm) |
CuSn7Zn4Pb7-C (CC493K) |
CuSn12-C (CC483K) |
ca kg/m |
76 | 75 | ✔ | ✔ | 40,3 |
81 | 80 | ✔ | ✔ | 45,8 |
86 | 85 | ✔ | ✔ | 51,6 |
91 | 90 | ✔ | ✔ | 57,8 |
96 | 95 | ✔ | ✔ | 64,4 |
102 | 100 | ✔ | ✔ | 73,0 |
107 | 105 | ✔ | 80,0 | |
112 | 110 | ✔ | ✔ | 88,0 |
117 | 115 | ✔ | 95,5 | |
levermaat (mm) |
schone maat (mm) |
CuSn7Zn4Pb7-C (CC493K) |
CuSn12-C (CC483K) |
ca kg/m |
122 | 120 | ✔ | ✔ | 104,0 |
127 | 125 | ✔ | 112,5 | |
132 | 130 | ✔ | ✔ | 122,0 |
142 | 140 | ✔ | ✔ | 141,0 |
152 | 150 | ✔ | ✔ | 161,5 |
162 | 160 | ✔ | ✔ | 183,4 |
172 | 170 | ✔ | ✔ | 206,7 |
182 | 180 | ✔ | ✔ | 231,4 |
192 | 190 | ✔ | ✔ | 259,3 |
levermaat (mm) |
schone maat (mm) |
CuSn7Zn4Pb7-C (CC493K) |
CuSn12-C (CC483K) |
ca kg/m |
202 | 200 | ✔ | ✔ | 285,2 |
212 | 210 | ✔ | ✔ | 317,0 |
222 | 220 | ✔ | ✔ | 348,0 |
232 | 230 | ✔ | ✔ | 380,0 |
242 | 240 | ✔ | ✚ | 413,0 |
252 | 250 | ✔ | ✔ | 447,0 |
262 | 260 | ✔ | 484,0 | |
272 | 270 | ✚ | ✚ | 521,0 |
282 | 280 | ✔ | ✔ | 560,0 |
levermaat (mm) |
schone maat (mm) |
CuSn7Zn4Pb7-C (CC493K) |
CuSn12-C (CC483K) |
ca kg/m |
304 | 300 | ✔ | ✔ | 650,0 |
334 | 330 | ✔ | 785,0 | |
354 | 350 | ✔ | ✔ | 881,0 |
404 | 400 | ✔ | ✔ | 1147,0 |
454 | 450 | ✔ | ✔ | 1464,1 |
✔ standaard | ✚ niet standaard, wel voorradig
2023-09-23 13:05
|
Toleranties | Buiten | Binnen |
---|---|---|
t/m Ø 117 mm | + 0 / + 1 mm | - 0 / - 1 mm |
Ø 122 - Ø 202 mm | + 0 / + 1,5 mm | - 0 / - 1,5 mm |
Ø 212 - Ø 504 mm | + 0 / + 2 mm | - 0 / - 2 mm |
vierkant en rechthoek | + 0 / +2 mm | |
Onze gieterijen kunnen centrifugaal gegoten (kraag)bussen fabriceren op iedere gewenste maat tot een diameter van maximaal Ø 2000 mm en lengten van 3000 mm in alle gangbare legeringen. |
EN | DIN | ||||
Benaming | CuSn7Zn4Pb7-C | CuSn7ZnPb | |||
Roepnaam | RG7 | ||||
Norm | EN 1982 | DIN 1705 | |||
Werkstofnr | CC493K | 2.1090 | |||
Chemische samenstelling | Mechanische eigenschappen | ||||
Cu | 81,0 - 85,0 | 81,0 - 85,0 | EN | DIN | |
Sn | 5,4 - 8,0 | 5,6 - 8,0 | Rm | ≥ 260 | ≥ 270 |
Zn | 2,0 - 5,0 | 3,0 - 5,0 | Rp 0,2 | ≥ 120 | ≥ 120 |
Pb | 5,0 - 8,0 | 5,0 - 7,0 | A5 | ≥ 12 | ≥ 16 |
Ni | 2,0 max. | 2,0 max. | HB | ≥ 70 | ≥ 70 |
P | 0,10 max. | 0,05 max. | |||
kg/dm³ | 8,9 | ||||
Uitvoering | GC, GZ | GC | |||
Kenmerken | Meest gangbare bronslegering, ook wel lagerbrons genoemd. Geschikt voor lagers met een middelmatige belasting, goede noodloopeigenschappen, hoge slijtvastheid en goed te verspanen. Algemene toepassingen: cylinder- en lagervoeringen, tandwielen en glijstrips. Belastingen tot 4000 N/cm². |
EN | DIN | ||||
Benaming | CuSn12-C | CuSn12 | |||
Roepnaam | Gbz12 | ||||
Norm | EN 1982 | DIN 1705 | |||
Werkstofnr | CC483K | 2.1052 | |||
Chemische samenstelling | Mechanische eigenschappen | ||||
Cu | 85,0 - 88,5 | 84,0 - 88,5 | EN | DIN | |
Sn | 10,5 - 13,0 | 10,5 - 13,0 | Rm | ≥ 300 | ≥ 280 |
Zn | 0,5 max. | 1,0 max. | Rp 0,2 | ≥ 150 | ≥ 140 |
Pb | 0,7 max. | 1,0 max. | A5 | ≥ 6 | ≥ 8 |
Ni | 2,0 max. | 2,0 max. | HB | ≥ 90 | ≥ 90 |
P | 0,60 max. | 0,4 max. | |||
kg/dm³ | ca. 8,9 | ||||
Uitvoering | GC, GZ | GC | |||
Kenmerken | Corrosie en zeewaterbestendig, goede slijtvastheid en bestand tegen hoge vlaktedrukken. Hogere mechanische waarden dan RG7 door meer tin en een lager lood- en zinkgehalte. Hierdoor zijn de noodloopeigenschappen en bewerkbaarheid wat minder. Toepassingen: lagers met hoge omtreksnelheden, zwaar belaste worm- en tandwielen, koppelingsonderdelen en draadbussen. |
EN | DIN | ||||
Benaming | CuSn5Zn5Pb5-C | CuSn5ZnPb | |||
Roepnaam | RG5 | ||||
Norm | EN 1982 | DIN 1705 | |||
Werkstofnr | CC491K | 2.1096 | |||
Chemische samenstelling | Mechanische eigenschappen | ||||
Cu | 83,0 - 87,0 | 84,0 - 86,0 | EN | DIN | |
Sn | 4,0 - 6,0 | 4,0 - 6,0 | Rm | ≥ 250 | ≥ 220 |
Zn | 4,0 - 6,0 | 4,0 - 6,0 | Rp 0,2 | ≥ 110 | ≥ 90 |
Pb | 4,0 - 6,0 | 4,0 - 6,0 | A5 | ≥ 13 | ≥ 16 |
Ni | 2,0 max. | 2,5 max. | HB | ≥ 65 | ≥ 60 |
P | 0,10 max. | ||||
kg/dm³ | 8,7 | ||||
Uitvoering | GC, GZ | GS | |||
Kenmerken | Wordt tegenwoordig meestal vervangen door RG7. |
EN | DIN | ||||
Benaming | niet genormeerd | CuSn10Zn | |||
Roepnaam | RG10 | ||||
Norm | DIN 1705 | ||||
Werkstofnr | 2.1086 | ||||
Chemische samenstelling | Mechanische eigenschappen | ||||
Cu | 86,0 - 89,0 | DIN | |||
Sn | 9,0 - 11,0 | Rm | ≥ 260 | ||
Zn | 1,0 - 3,0 | Rp 0,2 | ≥ 130 | ||
Pb | 1,5 max. | A5 | ≥ 15 | ||
Ni | 2,0 max. | HB | ≥ 77 | ||
P | 0,05 max. | ||||
kg/dm³ | 8,7 | ||||
Uitvoering | GC, GZ en GS |
EN | DIN | ||||
Benaming | CuSn10-C | CuSn10 | |||
Norm | EN 1982 | DIN 1705 | |||
Werkstofnr | CC480K | 2.1050 | |||
Chemische samenstelling | Mechanische eigenschappen | ||||
Cu | 88,0 - 90,0 | 88,0 - 90,0 | EN | DIN | |
Sn | 9,0 - 11,0 | 9,0 - 11,0 | Rm | ≥ 280 | ≥ 270 |
Zn | 0,5 max. | 0,5 max. | Rp 0,2 | ≥ 170 | ≥ 130 |
Pb | 1,0 max. | 1,0 max. | A5 | ≥ 10 | ≥ 18 |
Ni | 2,0 max. | 2,0 max. | HB | ≥ 80 | ≥ 70 |
P | 0,2 max. | 0,2 max. | |||
kg/dm³ | ca. 8,7 | ||||
Uitvoering | GS, GC, GZ | GS | |||
Kenmerken | Constructiemateriaal met hogere rek, corrosie- en zeewaterbestendigheid. |
EN | DIN | ||||
Benaming | CuSn12Ni2-C | CuSn12Ni | |||
Roepnaam | Gbz12Ni | ||||
Norm | EN 1982 | DIN 1705 | |||
Werkstofnr | CC484K | 2.1060 | |||
Chemische samenstelling | Mechanische eigenschappen | ||||
Cu | 84,5 - 87,5 | 84,0 - 87,0 | EN | DIN | |
Sn | 11,0 - 13,0 | 11,0 - 13,0 | Rm | ≥ 300 | ≥ 300 |
Zn | 0,4 max. | 0,4 max. | Rp 0,2 | ≥ 180 | ≥ 170 |
Pb | 0,3 max. | 0,3 max. | A5 | ≥ 10 | ≥ 10 |
Ni | 1,5 - 2,5 | 1,5 - 2,5 | HB | ≥ 95 | ≥ 90 |
P | 0,05 - 0,40 | 0,2 max. | |||
kg/dm³ | 8,6 | ||||
Uitvoering | GC, GZ | GC | |||
Kenmerken | Goede slijtvastheid, corrosie en zeewaterbestendig. Toepassingen zijn hoog belaste spindelmoeren, snellopende tand- en wormwielen. |
EN | DIN | ||||
Benaming | CuSn11Pb2-C | CuSn12Pb | |||
Roepnaam | Gbz12Pb | ||||
Norm | EN 1982 | DIN 1705 | |||
Werkstofnr | CC482K | 2.1061 | |||
Chemische samenstelling | Mechanische eigenschappen | ||||
Cu | 83,5 - 87,0 | 84,0 - 87,0 | EN | DIN | |
Sn | 10,5 - 12,5 | 11,0 - 13,0 | Rm | ≥ 280 | ≥ 280 |
Zn | 2,0 max. | 1,0 max. | Rp 0,2 | ≥ 150 | ≥ 140 |
Pb | 0,7 - 2,5 | 1,0 - 2,0 | A5 | ≥ 5 | ≥ 7 |
Ni | 2,0 max. | 2,0 max. | HB | ≥ 90 | ≥ 85 |
P | 0,4 max. | 0,2 max. | |||
kg/dm³ | 8,7 | ||||
Uitvoering | GC, GZ | GC | |||
Kenmerken | CuSn11Pb heeft in vergelijking met CuSn12 betere noodloopeigenschappen. Goede slijtvastheid, corriesie en zeewaterbestendig. Toepassingen zijn lagers met een hoge stootbelasting en leibaan-profielen. |